We used to grind the prep and finish it off with a file. It lets the bronze
penetrate in a bit.
Ray Freeman
-----Original Message-----
From: sel-bounces at lists.stationary-engine.com
[mailto:sel-bounces at lists.stationary-engine.com] On Behalf Of
Germoamer at aol.com
Sent: Sunday, 25 January 2009 11:26 PM
To: sel at lists.stationary-engine.com
Subject: Re: [SEL] Cracked Head/Vee grinding
In a message dated 1/24/2009 1:50:53 PM Eastern Standard Time,
jerrye at databak.co.za writes:
I'm no expert but have always been told NOT to use a grinder (of
the abrasive type) to vee out a groove for cast iron welding as the
abrasive (carborundum??) particles left behind in the metal may cause
problems with the weld. I've always been told to only use a file!
Jerry,
You are correct in not using abrasive type grinding tips to clean up metal
for epoxy repairs. What I have are a couple of air die grinders and use
high
speed/carbide cutting tips to do the work.
Tom Schmutz
Concord, Va.
germoamer at AOL.com
**************A Good Credit Score is 700 or Above. See yours in just 2 easy
steps!
(http://pr.atwola.com/promoclk/100000075x1215855013x1201028747/aol?redir=htt
p://www.freecreditreport.com/pm/default.aspx?sc=668072%26hmpgID=62%26bcd=De
cemailfooterNO62)
_______________________________________________
SEL mailing list
SEL at lists.stationary-engine.com
http://www.stationary-engine.com/mailman/listinfo/sel
More information about the sel
mailing list