[SEL] Cracked Head/Vee grinding
Germoamer at aol.com
Germoamer at aol.com
Sun Jan 25 06:46:49 PST 2009
In a message dated 1/24/2009 1:50:53 PM Eastern Standard Time,
jerrye at databak.co.za writes:
I'm no expert but have always been told NOT to use a grinder (of
the abrasive type) to vee out a groove for cast iron welding as the
abrasive (carborundum??) particles left behind in the metal may cause
problems with the weld. I've always been told to only use a file!
Jerry,
I use a lot of small carbide burrs much like:
http://cgi.ebay.com/CARBIDE-BURRS-100-PCS-1-8-MIXED-LOT_W0QQitemZ320334215185Q
QcmdZViewItemQQptZLH_DefaultDomain_0?hash=item320334215185&_trksid=p3911.c0.m1
4&_trkparms=72%3A1205%7C66%3A2%7C65%3A12%7C39%3A1%7C240%3A1318
Tom Schmutz
Concord, Va.
germoamer at AOL.com
**************A Good Credit Score is 700 or Above. See yours in just 2 easy
steps!
(http://pr.atwola.com/promoclk/100000075x1215855013x1201028747/aol?redir=http://www.freecreditreport.com/pm/default.aspx?sc=668072%26hmpgID=62%26bcd=De
cemailfooterNO62)
More information about the sel
mailing list